|  | During processing Ceramer can withstand very high temperatures even over long periods. 
 
 | 
																		
																			|  | At 320 °C over a period of 12 hours the weight loss is less than 1% (curve d). 
 
 | 
																		
																			|  | At 360 °C over a period of 12 hours the weight loss is only 4% (curve b). 
 
 | 
																		
																			|  | Curve a shows the weight loss at the recommended pre-treatment temperature of 375 °C, if Ceramer is used in free sintering of large volume parts. The drying duration is usually 330 minutes. The drying atmosphere is circulating air in a covered but vented container. 
 
 |